Convincing values and characteristics.

Coat Properties

CoatRecommended layer thickness 1) μmwith corrosion exposure
MildModerateStrongVery strong
KANIGEN®< 102550≥ 50
KANIGEN®
Heat treated 290 °C
< 102550≥ 50
KANISIL®
Heat treated 290 °C
102540≥ 50
KANISIL®PLUS203040≥ 50
KANICHROM®203050≥ 60
KANIFLON®< 101525≥ 40
Hard chrome 3)< 2020 – 30> 50ca. 100

____

Coat

Salt spray test

Attainable no. of hours according to SS DIN 50021

Kesternich test

SFW 2.S DIN 50018 attainable no. of cyclesl

Abrasionresistance

Taber 1,000 g/ 1,000 U

Surfacehardness

HV 0.05

KANIGEN®2) 1,00089.6560 – 580
KANIGEN®
Heat treated 290 °C
70064.5ca. 1,000
KANISIL®
Heat treated 290 °C
70060.6 – 0.8bis 1,200
KANISIL®PLUS2,000100.8 – 1.2bis 1,200
KANICHROM®2) 2,000101 – 2ca. 1,000
KANIFLON®8008-350 – 450
Hard chrome 3)120101 – 2ca 1,000


1) We precipitate the layers of the KANIGEN® group with a tolerance of up to ±2 %.
2) The coats have been tested for a number of years in seawater.
3) According to the tolerance range, the precision is achieved by additional mechanical processing.

Download & help

All information on this product can be found summarized for download in a PDF:

PDF-Download →

If you have questions, suggestions or requests? Then contact us equal. We are glad to be here for you.

Sonja Beisler
- Sales Assistant -

Phone:  +49 6021 709-0
E-Mail: info@schnarr.eu

Our office hours are:
Mon - Thu: 8:00am - 4:00pm
Fri: 8:00am - 1:30pm

    We call you back!
    Just leave your name and phone number please.